Durability Studies on Fly Ash Based Geopolymer Concrete ... Hindawi
The proportions of coarse aggregate, superplasticizer, and alkaliactivated solutions used in the geopolymer concrete mixes were 1189 kg/m 3, kg/m 3, and 171 kg/m 3, coarse aggregate and water used in the conventional concrete mix were 1189 kg/m 3 and 171 kg/m 3, Table 3, it is observed that G20M0 indicates that the mixes have 20% GGBS, 80% fly ash, and 0 ...